Please use this identifier to cite or link to this item:
http://cmuir.cmu.ac.th/jspui/handle/6653943832/71898
Full metadata record
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Punyada Intapibool | en_US |
dc.contributor.author | Naruporn Monmaturapoj | en_US |
dc.contributor.author | Katanchalee Nampuksa | en_US |
dc.contributor.author | Kriangkrai Thongkorn | en_US |
dc.contributor.author | Pathawee Khongkhunthian | en_US |
dc.date.accessioned | 2021-01-27T04:17:12Z | - |
dc.date.available | 2021-01-27T04:17:12Z | - |
dc.date.issued | 2021-01-01 | en_US |
dc.identifier.issn | 20574347 | en_US |
dc.identifier.other | 2-s2.0-85099096704 | en_US |
dc.identifier.other | 10.1002/cre2.394 | en_US |
dc.identifier.uri | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85099096704&origin=inward | en_US |
dc.identifier.uri | http://cmuir.cmu.ac.th/jspui/handle/6653943832/71898 | - |
dc.description.abstract | © 2021 The Authors. Clinical and Experimental Dental Research published by John Wiley & Sons Ltd. Background: Polymeric sponge technique is recommended for developing the desired porosity of Biphasic calcium phosphate (BCP) which may favor bone regeneration. Purpose: To investigate the healing of BCP with ratio of HA30/β-TCP70 (HA30) and HA70/β-TCP30 (HA70) polymeric sponge preparation, compare to commercial BCP (MBCP+TM). Materials and Methods: Materials were tested X-ray diffraction (XRD) pattern and scanning electron microscope (SEM) analysis. In eight male pigs, six calvarial defects were created in each subject. The defects were the filled with 1 cc of autogenous bone, MBCP+TM (MBCP), HA30, HA70, and left empty (negative group). The new bone formations, residual material particles and bone-to-graft contacts were analyzed at 4, 8, 12 and 16 weeks. Results: Fabricated BCP showed well-distributed porosity. At 16 weeks, new bone formations were 45.26% (autogenous), 33.52% (MBCP), 24.34% (HA30), 19.43% (HA70) and 3.37% (negative). Residual material particles were 1.88% (autogenous), 17.58% (MBCP), 26.74% (HA30) and 37.03% (HA70). These values were not significant differences (Bonferroni correction <0.005). Bone-to-graft contacts were 73.68% (MBCP), which was significantly higher than 41.68% (HA30) and 14.32% (HA70; Bonferroni correction <0.017). Conclusions: Polymeric sponge technique offers well-distributed porosity. The new bone formation and residual material particles were comparable to MBCP+TM, but the bone-to-graft contact was lower than MBCP+TM. | en_US |
dc.subject | Dentistry | en_US |
dc.title | Bone regeneration of a polymeric sponge technique—Alloplastic bone substitute materials compared with a commercial synthetic bone material (MBCP+TM technology): A histomorphometric study in porcine skull | en_US |
dc.type | Journal | en_US |
article.title.sourcetitle | Clinical and Experimental Dental Research | en_US |
article.stream.affiliations | Thailand National Science and Technology Development Agency | en_US |
article.stream.affiliations | Chiang Mai University | en_US |
Appears in Collections: | CMUL: Journal Articles |
Files in This Item:
There are no files associated with this item.
Items in CMUIR are protected by copyright, with all rights reserved, unless otherwise indicated.