Please use this identifier to cite or link to this item: http://cmuir.cmu.ac.th/jspui/handle/6653943832/65468
Full metadata record
DC FieldValueLanguage
dc.contributor.authorPetr Mikesen_US
dc.contributor.authorJana Horakovaen_US
dc.contributor.authorAles Samanen_US
dc.contributor.authorLucie Vejsadovaen_US
dc.contributor.authorPaul Tophamen_US
dc.contributor.authorWinita Punyodomen_US
dc.contributor.authorManita Dumklangen_US
dc.contributor.authorVera Jencovaen_US
dc.date.accessioned2019-08-05T04:33:48Z-
dc.date.available2019-08-05T04:33:48Z-
dc.date.issued2019-01-01en_US
dc.identifier.issn15308057en_US
dc.identifier.issn15280837en_US
dc.identifier.other2-s2.0-85065647038en_US
dc.identifier.other10.1177/1528083719848155en_US
dc.identifier.urihttps://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85065647038&origin=inwarden_US
dc.identifier.urihttp://cmuir.cmu.ac.th/jspui/handle/6653943832/65468-
dc.description.abstract© The Author(s) 2019. The study focuses on a comparison of the electrospinning of various polylactide and polycaprolactone (PLCL) copolymers and poly-L-lactide (PLLA) and polycaprolactone (PCL) homopolymers. The chemical characterisation, electrospinnability, fibrous morphology, degradation rate and interactions with fibroblasts were assessed with respect to copolymers and homopolymers with both lower (around 50,000) and higher (around 95,000) molecular weights. The research investigated commercially available as well as synthesised copolymers. The results revealed that the electrospinnability of polymeric solutions depends on both the molecular weight and the PLA/PCL ratio in the final copolymer. It was determined that PLCL copolymers with a higher content of PCL (≥20%) were not spinnable via the electrospinning process. With the exception of PCL, the resulting fibrous materials were found to be homogeneous and with fibre diameters of slightly more than 1 µm with respect to both the tested molecular weights. The degradation rate was tested under simulation conditions via the utilisation of the lipase and Proteinase K enzymes. The degree of degradation was found to depend on the molecular weight, the crystallinity of the polymer and the specificity of the enzyme applied. While lipase was responsible for the degradation of the PCL polymer, it exerted a minor impact on the PLLA and the copolymers. Proteinase K degraded all the tested polymers with a higher specificity towards PLLA and the PLCL copolymers. All the tested polymers were affected by the surface erosion degradation process via fibrous morphology changes and mass loss with no accompanying shift in the molar mass. The electrospun PLLA materials supported both fibroblast adhesion and proliferation. All the tested materials were determined to be cytocompatible with 3T3 mouse fibroblasts.en_US
dc.subjectChemical Engineeringen_US
dc.subjectEngineeringen_US
dc.subjectMaterials Scienceen_US
dc.titleComparison and characterization of different polyester nano/micro fibres for use in tissue engineering applicationsen_US
dc.typeJournalen_US
article.title.sourcetitleJournal of Industrial Textilesen_US
article.stream.affiliationsRajamangala University of Technology Lannaen_US
article.stream.affiliationsTechnická univerzita v Libercien_US
article.stream.affiliationsAston Universityen_US
article.stream.affiliationsChiang Mai Universityen_US
Appears in Collections:CMUL: Journal Articles

Files in This Item:
There are no files associated with this item.


Items in CMUIR are protected by copyright, with all rights reserved, unless otherwise indicated.