Please use this identifier to cite or link to this item:
http://cmuir.cmu.ac.th/jspui/handle/6653943832/63994
Full metadata record
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Jan Dutkiewicz | en_US |
dc.contributor.author | ukasz Rogal | en_US |
dc.contributor.author | P. Bobrowski | en_US |
dc.contributor.author | Magorzata Szutkowska | en_US |
dc.contributor.author | Wojciech Leniewski | en_US |
dc.contributor.author | Piotr Duzews | en_US |
dc.date.accessioned | 2019-05-07T09:59:42Z | - |
dc.date.available | 2019-05-07T09:59:42Z | - |
dc.date.issued | 2017 | en_US |
dc.identifier.issn | 0125-2526 | en_US |
dc.identifier.uri | http://it.science.cmu.ac.th/ejournal/dl.php?journal_id=8497 | en_US |
dc.identifier.uri | http://cmuir.cmu.ac.th/jspui/handle/6653943832/63994 | - |
dc.description.abstract | WC-Co composites with TiC additions of 5-20 wt.% substituting WC were consolidated using Hot Isostatic Pressing (HIP) method at temperature of 1350°C and pressure between 50-150 MPa. The hardness of WC-Co consolidated samples increase from 1050 HV (without TiC consolidated at 50 MPa) up to 1330 HV at 5% TiC and up to 1600 HV with 20% of TiC. The higher hardness of samples with TiC additions can be explained by a higher consolidation pressure of 150 MPa leading to a lower porosity, but also to hardening due to TiC addition. Young modulus values are lower for samples with TiC attaining 420-490 GPa as compared to 570 GPa for conventional WC-Co samples. Samples with a crack formation behavior allowed to determine fracture toughness KIC using crack length from hardness measurements. Results in the range 10, 9-11, 2 [MPam1/2] for the samples containing 0-10 % TiC, indicated only insignificant decrease of this property with TiC content. Addition of TiC causes also 15-30 % lower density of composites in the range 10-12, 5 g/cm3. The major identified phase is the hexagonal WC carbide separated by a narrow layer of Co binder and accompanied by single particles of TiC within Co. The size of WC particles was the same as applied in conventional composites i.e. 2-4 mm, while that of homogeneously distributed TiC were measured as slightly smaller, below 2 mm. Transmission electron microscopy investigations allowed to identify relatively high dislocation density in both cubic TiC and hexagonal WC carbides and different interfaces between WC and TiC carbides and Co binder however no additional phases were detected there. The crystallographic relationship [01-1] TiC || [100] WC was often observed. The appearance of solid solution of TiC with WC near WC/TiC interfaces was discussed. | en_US |
dc.language | Eng | en_US |
dc.publisher | Science Faculty of Chiang Mai University | en_US |
dc.title | The Effect of Substitution of WC by TiC in WC-Co Composite Tool Materials on Microstructure and Mechanical Properties | en_US |
dc.type | บทความวารสาร | en_US |
article.title.sourcetitle | Chiang Mai Journal of Science | en_US |
article.volume | 44 | en_US |
article.stream.affiliations | Institute of Metallurgy and Materials Science Polish Academy of Sciences 30-059 Krak w ul. Reymonta 25 Poland. | en_US |
article.stream.affiliations | Institute of Advanced Manufacturing Technology 30-011 Krak w, ul. Wroc awska 37a, Poland. | en_US |
article.stream.affiliations | Foundry Research Institute 30-418 Krak w ul. Zakopia ska 73, Poland. | en_US |
article.stream.affiliations | Institute of Physics of the Polish Academy of Sciences al. Lotnik w 32/46, 02-668 Warszawa, Poland. | en_US |
Appears in Collections: | CMUL: Journal Articles |
Files in This Item:
There are no files associated with this item.
Items in CMUIR are protected by copyright, with all rights reserved, unless otherwise indicated.