Please use this identifier to cite or link to this item:
http://cmuir.cmu.ac.th/jspui/handle/6653943832/57193
Full metadata record
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Yukari Noda | en_US |
dc.contributor.author | Masatoshi Nakajima | en_US |
dc.contributor.author | Masahiro Takahashi | en_US |
dc.contributor.author | Teerapong Mamanee | en_US |
dc.contributor.author | Keiichi Hosaka | en_US |
dc.contributor.author | Tomohiro Takagaki | en_US |
dc.contributor.author | Masaomi Ikeda | en_US |
dc.contributor.author | Richard M. Foxton | en_US |
dc.contributor.author | Junji Tagami | en_US |
dc.date.accessioned | 2018-09-05T03:36:17Z | - |
dc.date.available | 2018-09-05T03:36:17Z | - |
dc.date.issued | 2017-01-01 | en_US |
dc.identifier.issn | 18811361 | en_US |
dc.identifier.issn | 02874547 | en_US |
dc.identifier.other | 2-s2.0-85037548772 | en_US |
dc.identifier.other | 10.4012/dmj.2016-383 | en_US |
dc.identifier.uri | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85037548772&origin=inward | en_US |
dc.identifier.uri | http://cmuir.cmu.ac.th/jspui/handle/6653943832/57193 | - |
dc.description.abstract | © 2017, Japanese Society for Dental Materials and Devices. All rights reserved. This study evaluated the effects of ceramic surface treatment agents on shear bond strengths to ceramic materials with and without thermocycling. Ceramic plates were prepared from feldspathic ceramic; AAA, lithium disilicate ceramic material; IPS e.max Press, zirconia ceramic; Lava. Ceramic surfaces were pretreated with one of five surface treatment agents (Clearfil PhotoBond mixed with Porcelainbond activator (PB), Clearfil SE One mixed with Porcelainbond activator (SO), Ceramic Primer (CP), Universal Primer (UP), Scotchbond Universal (SU)), and then a resin cement (Clapearl DC) was filled. After 0, 5,000, and 10,000 thermocycles, micro-shear bond strengths between ceramic-cement interfaces were determined. SU exhibited significantly lower initial bond strength to AAA and e.max than PB, SO, CP, and UP. For Lava, PB, SO, CP and SU exhibited higher initial bond strengths than UP. Thermocycles reduced bond strengths to all the ceramic materials with any surface treatment. | en_US |
dc.subject | Dentistry | en_US |
dc.subject | Materials Science | en_US |
dc.title | The effect of five kinds of surface treatment agents on the bond strength to various ceramics with thermocycle aging | en_US |
dc.type | Journal | en_US |
article.title.sourcetitle | Dental Materials Journal | en_US |
article.volume | 36 | en_US |
article.stream.affiliations | Tokyo Medical and Dental University | en_US |
article.stream.affiliations | Chiang Mai University | en_US |
article.stream.affiliations | King's College London | en_US |
Appears in Collections: | CMUL: Journal Articles |
Files in This Item:
There are no files associated with this item.
Items in CMUIR are protected by copyright, with all rights reserved, unless otherwise indicated.