Please use this identifier to cite or link to this item:
http://cmuir.cmu.ac.th/jspui/handle/6653943832/77674
Full metadata record
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Piewpan Parjansri | en_US |
dc.contributor.author | Sukum Eittsayeam | en_US |
dc.contributor.author | Kamonpan Pengpat | en_US |
dc.date.accessioned | 2022-10-16T08:14:12Z | - |
dc.date.available | 2022-10-16T08:14:12Z | - |
dc.date.issued | 2020-01-01 | en_US |
dc.identifier.issn | 16078489 | en_US |
dc.identifier.issn | 10584587 | en_US |
dc.identifier.other | 2-s2.0-85102973380 | en_US |
dc.identifier.other | 10.1080/10584587.2020.1857176 | en_US |
dc.identifier.uri | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85102973380&origin=inward | en_US |
dc.identifier.uri | http://cmuir.cmu.ac.th/jspui/handle/6653943832/77674 | - |
dc.description.abstract | (Bi0.5Na0.5)TiO3 (BNT) lead-free ceramics were prepared by the seed-induced technique using different particle sizes of BaTiO3 (BT) powder as seeds. The BT seeds was synthesized by the molten-salt method and then calcined at different temperatures of 750 (750BTs), 800 (800BTs) and 850 °C (850BTs). The pure perovskite seeds (5 mol%) were mixed with the starting materials of the BNT system for conventional mixed oxide method. After that, the mixture was calcined and sintered at 900 °C for 2 h and 1100 °C for 2 h, respectively. From results it was found that the particle size of BT seed increased with calcine temperature increase from 750 to 850 C. The samples of non-BT seed (S0) and BT seed-added (S1, S2 and S3) showed pure perovskite phase. Average density values were in the range of 5.53-5.77 g/cm3. Dielectric constant (εr) measured at room temperature (at 1 kHz) was in the range of 732.04-788.59. The dielectric loss (tanδ), remnant polarization (Pr) and coercive field (Ec) values decreased with the addition of BT seed. The highest piezoelectric coefficient (d33) ∼156 pC/N was obtained for the sample of 850BTs (S3). | en_US |
dc.subject | Engineering | en_US |
dc.subject | Materials Science | en_US |
dc.subject | Physics and Astronomy | en_US |
dc.title | Improvement in Electrical Properties of (Bi<inf>0.5</inf>Na<inf>0.5</inf>)TiO<inf>3</inf> (BNT) Ceramics Using the Seed-Induced Method | en_US |
dc.type | Journal | en_US |
article.title.sourcetitle | Integrated Ferroelectrics | en_US |
article.volume | 214 | en_US |
article.stream.affiliations | Rajamangala University of Technology Krungthep | en_US |
article.stream.affiliations | Chiang Mai University | en_US |
Appears in Collections: | CMUL: Journal Articles |
Files in This Item:
There are no files associated with this item.
Items in CMUIR are protected by copyright, with all rights reserved, unless otherwise indicated.