Please use this identifier to cite or link to this item: http://cmuir.cmu.ac.th/jspui/handle/6653943832/74904
Full metadata record
DC FieldValueLanguage
dc.contributor.authorJerachard Kaimaen_US
dc.contributor.authorItthichai Preechawuttipongen_US
dc.contributor.authorRobert Peyrouxen_US
dc.contributor.authorPawarut Jongchansittoen_US
dc.contributor.authorCécile Sillarden_US
dc.contributor.authorJeremie Viguieen_US
dc.contributor.authorEvelyne Maureten_US
dc.date.accessioned2022-10-16T06:52:42Z-
dc.date.available2022-10-16T06:52:42Z-
dc.date.issued2022-08-01en_US
dc.identifier.issn16629752en_US
dc.identifier.issn02555476en_US
dc.identifier.other2-s2.0-85136277199en_US
dc.identifier.other10.4028/p-8oo3r9en_US
dc.identifier.urihttps://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85136277199&origin=inwarden_US
dc.identifier.urihttp://cmuir.cmu.ac.th/jspui/handle/6653943832/74904-
dc.description.abstractIn order to use bamboo as reinforcement in composite material, we first need to extract individual fibers from bamboo strips and re-fabricated as hand sheets. Those hand sheets contain millions of individual fibers contacting each other by their surface force and mainly hydrogen bonding. Therefore, different NaOH concentration used during the extraction stage would provide different surface properties impacting tensile strength of bamboo hand sheets. The objective of this study is to recommend suitable concentrations of NaOH for producing hand sheets as reinforcement material. Hand sheets were produced by cooked bamboo strips in different NaOH concentration, which are 1%, 6%, and 30% at 120o c for 2 hours. More than 10 samples of bamboo hand sheets with different treatments were submitted to mechanical tensile test following ISO 1924-1. It was found that the ultimate tensile strength and the Young’s modulus of bamboo hand sheets of the different specimen were globally similar. However, for low concentration, ultimate tensile strength and Young’s modulus increase while the NaOH concentration increases. On the other hand, higher values of NaOH concentration do not only extract bamboo fiber but also severely alter bamboo fiber shape. The best ultimate tensile strength and Young’s modulus values are presented by 6% NaOH which are 0.95 kN/m2 and 236.4 MPa respectively.en_US
dc.subjectEngineeringen_US
dc.subjectMaterials Scienceen_US
dc.titleEffect of NaOH Concentration on Tensile Strength of Bamboo Hand Sheeten_US
dc.typeBook Seriesen_US
article.title.sourcetitleMaterials Science Forumen_US
article.volume1067en_US
article.stream.affiliationsUniversite Grenoble Alpesen_US
article.stream.affiliationsChiang Mai Universityen_US
Appears in Collections:CMUL: Journal Articles

Files in This Item:
There are no files associated with this item.


Items in CMUIR are protected by copyright, with all rights reserved, unless otherwise indicated.