Please use this identifier to cite or link to this item: http://cmuir.cmu.ac.th/jspui/handle/6653943832/67881
Full metadata record
DC FieldValueLanguage
dc.contributor.authorPichitchai Butnoien_US
dc.contributor.authorSupalak Manothamen_US
dc.contributor.authorGobwute Rujijanagulen_US
dc.date.accessioned2020-04-02T15:08:56Z-
dc.date.available2020-04-02T15:08:56Z-
dc.date.issued2019-11-18en_US
dc.identifier.issn15635112en_US
dc.identifier.issn00150193en_US
dc.identifier.other2-s2.0-85075953769en_US
dc.identifier.other10.1080/00150193.2019.1653080en_US
dc.identifier.urihttps://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=85075953769&origin=inwarden_US
dc.identifier.urihttp://cmuir.cmu.ac.th/jspui/handle/6653943832/67881-
dc.description.abstract© 2019, © 2019 Taylor & Francis Group, LLC. In this present work, the effect of heating/coolling rate on the electrical properties such as ferroelectric, dielectric and electrostrictive properties of Pb-free Bi0.45La0.05Na0.40K0.10-Ti0.98Zr0.02O3 or BLNKZT piezoelectric ceramics has been systematically investigated. The BLNKZT ceramics were prepared via a conventional solid state reaction method and sintered at 1125 °C for 2 h, which applied the heating/cooling rates of 5, 10 and 15 °C/min in order to clarify the optimal parameter for densification and good electrical properties. The XRD pattern exhibited a complete single perovskite structure with a pseudo-cubic phase at the rate of 5 °C/min sample and tranformed to tetragonal-rich phase at the rate of 15 °C/min. The SEM micrograph of all BLNKZT ceramics showed a cubic-like grain shape. The P-E hysteresis loop was measured at the temperatures ranging from −40 to 120 °C. With increasing temperature, the Pr and Ec values distinctly decreased and the P-E loops tended to deform and showed pinch loops. The maximum strain (Smax) value of 0.10% and calculated normalized strain (d*33) of 167 pm/V (measured at 60 kV/cm) were obtained for ceramic sintered with the heating/cooling rates of 5 °C/min.en_US
dc.subjectMaterials Scienceen_US
dc.subjectPhysics and Astronomyen_US
dc.titleHeating rate effect on dielectric, ferroelectric and piezoelectric properties of Bi<inf>0.45</inf>La<inf>0.05</inf>Na<inf>0.40</inf>K<inf>0.10</inf>Ti<inf>0.98</inf>Zr<inf>0.02</inf>O<inf>3</inf> Pb-free piezoelectric ceramic for actuator applicationsen_US
dc.typeJournalen_US
article.title.sourcetitleFerroelectricsen_US
article.volume552en_US
article.stream.affiliationsChiang Mai Universityen_US
Appears in Collections:CMUL: Journal Articles

Files in This Item:
There are no files associated with this item.


Items in CMUIR are protected by copyright, with all rights reserved, unless otherwise indicated.