Title: Oxidation behavior of 30wt.%Cr-3.75wt.%V high chromium cast iron
Authors: Amporn Wiengmoon
Jeerapat Nakpratum
Torranin Chairuangsri
John T H Pearce
Authors: Amporn Wiengmoon
Jeerapat Nakpratum
Torranin Chairuangsri
John T H Pearce
Keywords: Engineering;Materials Science
Issue Date: 1-Jan-2016
Abstract: © 2016 Trans Tech Publications, Switzerland. This work focuses on the oxidation behavior of 2.4wt.%C-30wt.%Cr-3.75wt.%V cast iron in air at 1000 oC for 1-48 h with weight gain measurements taken at different times. The oxidized surfaces and cross sections were characterized by XRD, OM, SEM and EDS. It was found that the as-cast microstructure consisted of a ferritic matrix and M7C3carbide. The surface oxide scale consisted of multi-oxides and the grain size of the oxides increased with increasing holding times. XRD and SEM-EDS results revealed that the multi-oxide layer can be Cr2O3, (Fe,Cr,V)2O3and SiO2. After about 48 h, a continuous SiO2inner-layer was observed and the oxide scale tended to swell, contained pores, and became detached from the surface because of its poor adherence.
URI: https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84958211436&origin=inward
http://cmuir.cmu.ac.th/jspui/handle/6653943832/55833
ISSN: 10139826
Appears in Collections:CMUL: Journal Articles

Files in This Item:
There are no files associated with this item.


Items in CMUIR are protected by copyright, with all rights reserved, unless otherwise indicated.