Please use this identifier to cite or link to this item:
http://cmuir.cmu.ac.th/jspui/handle/6653943832/54620
Full metadata record
DC Field | Value | Language |
---|---|---|
dc.contributor.author | S. Imurai | en_US |
dc.contributor.author | Ch Thanachayanont | en_US |
dc.contributor.author | J. T.H. Pearce | en_US |
dc.contributor.author | T. Chairuangsri | en_US |
dc.date.accessioned | 2018-09-04T10:18:41Z | - |
dc.date.available | 2018-09-04T10:18:41Z | - |
dc.date.issued | 2015-01-01 | en_US |
dc.identifier.issn | 17333490 | en_US |
dc.identifier.other | 2-s2.0-84958207318 | en_US |
dc.identifier.other | 10.1515/amm-2015-0230 | en_US |
dc.identifier.uri | https://www.scopus.com/inward/record.uri?partnerID=HzOxMe3b&scp=84958207318&origin=inward | en_US |
dc.identifier.uri | http://cmuir.cmu.ac.th/jspui/handle/6653943832/54620 | - |
dc.description.abstract | Microstructure and erosion-corrosion behaviour of as-cast high chromium white irons containing molybdenum in aqueous sulfuric-acid slurry was studied. The experimental irons contained 28 wt.%Cr with a Cr:C ratio of about 10 and up to 10 wt.%Mo. The irons with up to 6 wt.%Mo are hypoeutectic, whereas the iron with 10 wt.%Mo becomes eutectic/peritectic. Mo addition promotes formation of M23C6and M6C, instead of typical M7C3. Erosion-corrosion testing was performed in aqueous sulfuric-acid slurry containing alumina particles. The hypoeutectic Fe-28Cr-2.7C-1Mo with mainly M7C3and the eutectic/peritectic Fe-28Cr-2.6C-10Mo showed reduced wear rates of about 30% and 7% of that of the reference iron without Mo addition, respectively. The reduction of the carbide-matrix hardness difference, the increase of corrosion resistance of the matrices, and the increase of macro-hardness are determining factors for the improvement of erosion-corrosion resistance of the irons. | en_US |
dc.subject | Materials Science | en_US |
dc.title | Microstructure and erosion-corrosion behaviour of as-cast high chromium white irons containing molybdenum in aqueous sulfuric-acid slurry | en_US |
dc.type | Journal | en_US |
article.title.sourcetitle | Archives of Metallurgy and Materials | en_US |
article.volume | 60 | en_US |
article.stream.affiliations | Chiang Mai University | en_US |
article.stream.affiliations | Thailand National Metal and Materials Technology Center | en_US |
article.stream.affiliations | Panyapiwat Institute of Management | en_US |
Appears in Collections: | CMUL: Journal Articles |